| Availability: | |
|---|---|
| Quantity: | |
Product Description
Hot Mounting Powder Comparison Chart
| Name | PR Mounting Powder | GC Mounting Powder | EP Mounting Powder | TM Mounting Powder |
| Heat time | 4~6 mins | 4~6 mins | 4~6 mins | 25 mins |
| Cooling time | 2~3 mins | 4~6 mins | 2~3 mins | 15 mins |
| Pressure | 100~300 bar | 100~300 bar | 100~150 bar | 150 bar |
| Heat TEMP | 150~180 °C | 150~180 °C | 140~180˚C | 140±5 °C |
| Hardness | 85~90 Shore D | 90~92 Shore D | 90~93 Shore D | 85~87 Shore D |
*Date is based on the diameter of 30 mm heating mold, for reference only.
PR-B/G/R Phenolic Resin Hot Mounting Powder
| Application: For routine applications suit for most products. | ![]() | ![]() |
Material: Phenolic resin, bakelite powder. | ![]() | |
| Technical Specification | ||
| Color: Black, Green, Red | ||
| Package: 500g/Bottle, 2000g/Bottle, 4000g/Bottle, 18000g/Bottle | ||
GCB Graphite Conductivity Hot Mounting Powder
Application: Suitable for conductive samples such as: for electron microscopy, electrolytic polishing, SEM analysis | ![]() |
| Features: Excellent conductive, voltage loss almost eliminated completely. | |
| Technical Specification | |
| Color: Black | |
| Package: 500g/Bottle, 2000g/Bottle, 4000g/Bottle, 18000g/Bottle | |
EPB Edge Protection Hot Mounting Powder
Application: Samples with high edge requirements. | ![]() |
Features: Black color, extremely low shrinkage.Tightly combined with the sample, with high hardness,good abrasion resistance. | |
| Technical Specification | |
| Color: Black | |
| Package: 500g/Bottle, 2000g/Bottle, 4000g/Bottle, 18000g/Bottle | |
TM Transparent Acrylic Acid Hot Mounting Powder
Application: Complete embedding solution for thin layers, top layer for specimen labeling. | ![]() |
Features: Transparent and very clear.allows easy sample observation | |
| Technical Specification | |
| Color: White Powder | |
| Package: 500g/Bottle, 2000g/Bottle, 4000g/Bottle, 18000g/Bottle | |
Guidance for Hot Mounting Compound
Before sample mounting process, the grease on the sample needs to be removed so that the mounting resin can
perfectly adhere to the surface of the sample. If burrs are generated during the cutting process, you can use sandpaper to remove the burrs on the edge of the sample.
| Problem | Causes | Solutions |
| Bulge | Less cooling time |
|
| Primer cracks | Oversized Coated part according to the chosen mounting mould | Reduce the size of the sample or increase the size of the mounting mould |
| Shrinkage | Inadequate mounting resins | Choose less shrinkage resins |
| Insufficient heating time | Increase the temperature during the heating time | |
| Insufficient pressure | Increase the mounting pressure | |
| "Smoke" visible | Wrong pressure choice | Increase pressure only during cooling cycle |
| Too much resin than sample dimension | Reduce resin quantity or mold dimension | |
| Insufficient heating time | Increase the heating time | |
| Resins grains visible | Insufficient pressure | Increase the pressure during the mounting cycle |
| Insufficient heating time | Increase the heating time |